My prints get very good adhesion to the bed, especially when doing prints with large adhesion areas. So good, that after the print is done, I actually have to wet the surface with alcohol and put it in the freezer for it to let go!

My question is, if the adhesion could be a bit less violent, if I lower or increase the bed temperature? I have an ender 3 v2 with the original glass bed (it has some black layer on top of the glass).

I know that there are tons of alternative beds that I could buy, but I’d rather keep this bed if I can counter the too strong adhesion

  • rambos@lemm.ee
    link
    fedilink
    English
    arrow-up
    0
    ·
    9 months ago

    In my experience PLA just pops off the clean glass when cooled to room temp (holds extremely well if bed is at 45C or more). I have some tips, but only to improve adhesion xD You can maybe try less squish on the first layer (lower flow rate or increase nozzle distance a bit) or just use thin layer of glue. Too low or too high bed temp can ruin bed adhesion, but feels like wrong approach imo, still worth a try